X6NiCrTiMoVB25-15-2 datasheet,X6NiCrTiMoVB25-15-2 chemical,X6NiCrTiMoVB25-15-2 heat treatment
Home > Superalloy > Text

X6NiCrTiMoVB25-15-2
2019-05-31 09:13:15   Origin:   Remark:0 Click:

Material technical specification of high alloy X6NiCrTiMoVB25-15-2 datasheet,X6NiCrTiMoVB25-15-2 Chemical compositions, X6NiCrTiMoVB25-15-2 mechanical properties from Steelmaking, ESR melting, Hot blooming, 100% UT, Hot forging, Hot rolling, Heat treatment, Straightening, 100% Ultrasonic test, Cold working or Machined. Technical specifications - ISO / TR 4956 - 1984, 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

 

 
TECHNICAL DATA SHEET - Alloy X6NiCrTiMoVB25-15-2

OFFICIAL TEST CERTIFICATE: issued by TUV - SGS BV
MATERIAL CATEGORY: High temperature alloy steel for internal combustion engine
MATERIAL SPECIFICATIONS: ISO / TR 4956 - 1984
CHEMICAL COMPOSITION (WEIGHT %)
C (%):     0.03 ~ 0.08
Si (%):     ≤ 1.00
Mn (%):   ≤ 2.00
P (%)≤:   0.025
S (%)≤:   0.015
Cr (%):    13.5 ~ 16.0
Ni (%):     24.0 ~ 27.0
Mo (%):   1.00 ~ 1.50
V (%):      0.10 ~ 0.50
Ti (%):     1.90 ~ 2.30
B (%):      0.003 ~ 0.010 
MECHANICAL PROPERTIES UNDER ROOM TEMP.  
Condition of heat treatment: Quenched and tempered
Tensile strength, σb ≥/MPa: 900 ~ 1100
Yield strength, σ0.2 ≥/MPa: 600
Elontation, δ ≥(%): 15.0
Reduction of area, ф ≥(%): -
Hardness | HBW: 331 max.
FORMS AND SHAPES
Round bar (Diameter): 5.50 ~ 650mm
Square bar / Flat bar: 3 ~ 650mm Wire rod (Diameter): 0.10 ~ 16mm
Steel strip via cold rolled: T0.1 - 3mm X W5 - 650mm X L (or in coil form)
Forging piece: Different shapes based on OEM.

Hot search:X6NiCrTiMoVB25-15-2

Previous page:X12CrNiMoV12-2
Last page:最后一页