Aquamet 22 datasheet,Aquamet 22 chemical,Aquamet 22 heat treatment

Aquamet 22
2020-03-12 11:29:15   Origin:   Remark:0 Click:

Description Aquamet 22 Datasheet, Shaft Aquamet 22 Suppliers, Inventory Aquamet 22 Forging Bar Plate, Technical Specifications Melting, ESR & VAR technique, Hot blooming, Hot forging, Hot rolling, Heat treatment, Straightening, Ultrasonic flaw detection test.
MATERIAL DATA SHEET - Grade Aquamet 22

OFFICIAL TEST CERTIFICATE - issued by TUV - SGS -  BV
MATERIAL CATEGORY - Nonmagnetic special alloys
MELTING PROCESS - EAF + AOD / + ESR
H S CODE For Customs - 7228 4000 / 7228 5000 / 7228 6000
MATERIAL SHORT BRIEF - AQUAMET 22 is a high-alloy austenitic
stainless steel that provides superior corrosion resistance along with excellent toughness and high strength.
CHEMICAL COMPOSITION ( Mass Weight - % )
C (%):    ≤ 0.06
Si (%):    ≤ 1.00
Mn (%):  4.00 ~ 6.00
P (%)≤:  0.035
S (%)≤:  0.015
Cr (%):   20.5 ~ 23.5
Ni (%):   11.5 ~ 13.5
Mo (%):  1.50 ~ 3.00
Co (%):  -
W (%):   -
Al (%):   -
Nb (%):  0.10 ~ 0.30
Ti (%):    -
N (%):   0.20 ~ 0.40
V (%):    0.10 ~ 0.30
MECHANICAL PROPERTIES UNDER ROOM TEMP.
Tensile strength, σb/≥ MPa: 690
Yield strength, σ0.2/≥ MPa: 380
Elonghation, δ ≥(%): 18.0
Reduction of area, ф ≥ (%): 45.0
Hardness | HB:
AVAILABLE FORMS AND DIMENSIONS
Round bar & Shaft (Diameter): 5.5mm to 550mm
Square bar / Flat bar: 10mm to 500mm
Steel strip via cold rolled: T0.5 - 3mm X W5 - 200mm X L (or in coil form)
Forging piece & Shaft: Different shapes based on OEM.
TECHNICAL SALES ASSISTANCE AND SERVICE
If you meet further on any technical enquiry or help, pleased to EMAIL 